Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 2.20 g/micron | 56.0 g/mil | ASTM D1922 |
ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Extrusion Coating
(discontinued **) Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer designed for extrusion coating, laminating and seaming applications. It can be process.. |
|||
Elmendorf Tear Strength, TD | 2.20 g/micron | 56.0 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-333 EVA Film Resin, Very High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-333 exhibits superior impact strength, clarity and heat sealability.Applications: Prim.. |
|||
Elmendorf Tear Strength, TD | 2.20 g/micron | 56.0 g/mil | ASTM D1922 |
Dow 662I Low Density Polyethylene Resin Blown Film Resin designed for enhanced bubble stability High melt strength Optimum gauge range: 1.5 - 5.0 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow |
|||
Elmendorf Tear Strength, TD | 2.20 g/micron | 56.0 g/mil | ASTM D1922 |
Ashley Polymers Ashlene® 850 Nylon 6 This is an extrusion grade Nylon 6 resin suitable for both coextrusion and blown film applications. It has excellent melt stability and very high melt strength. It also has excellent grease resist.. |
|||
Elmendorf Tear Strength, TD | 2.20 g/micron | 56.0 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-331 EVA Film Resin, Very High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.8% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati.. |