Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 17.2 g/micron | 437 g/mil | ASTM D 1922 |
NOVA Chemicals Surpass® FPs016-C Octene sLLDPE Film Resin FPs016-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |
|||
Elmendorf Tear Strength, TD | 17.2 g/micron | 437 g/mil | ASTM-D1922 |
Braskem FC31D LLDPE Blown Film Extrusion Polyethylene Copolymer The FC31D resin is a linear low-density polyethylene, copolymer of butene -1, produced by the solution process for blow film extrusion. It has excellent mechanical properties, especially hot tack. I.. |