Polymer Property : Elmendorf Tear Strength, TD = 213 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 8.40 g/micron
213 g/mil
ISO 6383-2
Total HDPE HL 717 High Density Polyethylene - Blown Film
HDPE HL 717 is a high density polyethylene produced by the gas phase polymerization process with hexene as a comonomer.HDPE HL 717 is a monomodal HDPE with a broad molecular weight distribution. It..
Elmendorf Tear Strength, TD 8.40 g/micron
213 g/mil
Dow DOWLEX™ 2027A Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2027A Polyethylene resin is a higher density polymer for cast film applications with improved stiffness. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2(a) for food contact appli..