Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 5.6045 g/micron | 142.35 g/mil | ISO 6383-2 |
Polimeri Europa Greenflex® FF 55 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FF 55 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FF 55 show high flexibility.Main Applications: Greenflex FF 55 is recommended f.. |
|||
Elmendorf Tear Strength, TD | 5.6045 g/micron | 142.35 g/mil | ISO 6383-2 |
Polimeri Europa Riblene® FH 20 Low Density Polyethylene - Blown Film Extrusion Riblene FH 20 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FH 20 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
Elmendorf Tear Strength, TD | 5.6045 g/micron | 142.35 g/mil | ISO 6383-2 |
Polimeri Europa Riblene® FL 30 Low Density Polyethylene - Blown Film Extrusion Riblene FL 30 is a low density polyethylene (LDPE) ideal for blown film extrusion. Riblene FL 30 is characterized by a good balance between processability, mechanical and optical properties.Films m.. |
|||
Elmendorf Tear Strength, TD | 5.6045 g/micron | 142.35 g/mil | ISO 6383-2 |
Polimeri Europa Riblene® FM 34 Low Density Polyethylene - Blown Film Extrusion Riblene FM 34 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 is characterized by a good balance between processabilit.. |
|||
Elmendorf Tear Strength, TD | 5.6045 g/micron | 142.35 g/mil | ISO 6383-2 |
Polimeri Europa Riblene® FM 34 E Low Density Polyethylene - Blown Film Extrusion Riblene FM 34 E is a low density polyethylene (LDPE) with added slip (erucamide) and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 E is characterized by a good balance betwe.. |