Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 4.70 g/micron | 119 g/mil | ASTM D1922 |
Petroquimica Triunfo Trithene® CX 7065 LDPE - Extrusion Coating The Trithene® CX 7065 resin is a product developed especially to meet the segment of extrusion coating where the following properties are necessary: processing stability at high production rates, a.. |
|||
Elmendorf Tear Strength, TD | 4.70 g/micron | 119 g/mil | ASTM D1922 |
Eastman E6838-899F Polyethylene
(discontinued **) E6838-899F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat-sealing range, and good pr.. |
|||
Elmendorf Tear Strength, TD | 4.69 g/micron | 119 g/mil | Calculated from mfr's report of 14.2 N per TAPPI-414 and the typical thickness |
DuPont™ Nomex® 410 Paper, 12 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Elmendorf Tear Strength, TD | 4.69 g/micron | 119 g/mil | Calculated from mfr's report of 23.7 N per TAPPI-414 and the typical thickness |
DuPont™ Nomex® 410 Paper, 20 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Elmendorf Tear Strength, TD | 4.70 g/micron | 119 g/mil | |
Dow AFFINITY™ HF 1030 Polyolefin Plastomer AFFINITY® HF 1030 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide cast embossed film products with high modulus for machinability, excellent drawdown at high line speeds,.. |
|||
Elmendorf Tear Strength, TD | 4.70 g/micron | 119 g/mil | |
Dow HDPE 05862N High Density Polyethylene Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical. |
|||
Elmendorf Tear Strength, TD | 4.67 g/micron | 119 g/mil | ASTM-D1922 |
Braskem TU3001 LDPE Blown Film Extrusion Polyethylene TU3001 is a low-density polyethylene (LDPE) with high molecular weight, excellent mechanical properties, and good processability. These qualities ensure the production of films with uniform thicknes.. |