Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 33.1 g/micron | 840 g/mil | Notched; ASTM D1992 |
Chevron Phillips MarFlex® 7109S LLDPE Blown Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Elmendorf Tear Strength, TD | 33.1 g/micron | 840 g/mil | ASTM D1922 |
Chevron Phillips 7109DT LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene Copolymer, No Slip, No Antiblock Version of 7109T with Process Aid, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or ble.. |
|||
Elmendorf Tear Strength, TD | 33.1 g/micron | 840 g/mil | ASTM D1922 |
Chevron Phillips 7109T LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Industrial Liners, Stretch Wrap, Garment Bags.. |
|||
Elmendorf Tear Strength, TD | 33.1 g/micron | 841 g/mil | ASTM D1922 |
Chevron Phillips 7109D Linear low density polyethylene blown film resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymer, no slip, no antiblock version of 7109 with process aid, cast/blown resinCharacteristics: good stiffness at thin gauges, good drawdown, .. |
|||
Elmendorf Tear Strength, TD | 33.1 g/micron | 840 g/mil | Notched; ASTM D1992 |
Chevron Phillips MarFlex® 7109 LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Elmendorf Tear Strength, TD | 33.1 g/micron | 840 g/mil | Notched; ASTM D1992 |
Chevron Phillips MarFlex® 7109DJ LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |