Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 31.5 g/micron | 800 g/mil | Notched; ASTM D1992 |
Chevron Phillips MarFlex® 7109L LLDPE Blown Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Elmendorf Tear Strength, TD | 31.5 g/micron | 800 g/mil | ASTM D1922 |
Chevron Phillips Vytek™ V205C6 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Elmendorf Tear Strength, TD | 31.5 g/micron | 800 g/mil | Notched; ASTM D1992 |
Chevron Phillips MarFlex® 7109DL LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Elmendorf Tear Strength, TD | 31.5 g/micron | 800 g/mil | Notched; ASTM D1992 |
Chevron Phillips MarFlex® 7109M LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Elmendorf Tear Strength, TD | 31.5 g/micron | 800 g/mil | ASTM D1922 |
Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HSE-7002 NT 7 is an ethylene-hexene-1 copolymer, design.. |
|||
Elmendorf Tear Strength, TD | 31.5 g/micron | 800 g/mil | Notched; ASTM D1992 |
Chevron Phillips MarFlex® 7109CL LLDPE Blown Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |