Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 3.20 g/micron | 81.3 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® LF-Y320-C Fractional Melt LDPE Film Resin Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL.. |
|||
Elmendorf Tear Strength, TD | 3.20 g/micron | 81.3 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® LF-Y320-D Fractional Melt LDPE Film Resin Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL.. |