Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 29.5 g/micron | 750 g/mil | ASTM D1922 |
ExxonMobil NTX™ NTX 095 Super Strength Film Resin NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac.. |
|||
Elmendorf Tear Strength, TD | 29.5 g/micron | 750 g/mil | ASTM D1922 |
ExxonMobil NTX™ NTX 104 Super Strength Film Resin NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac.. |
|||
Elmendorf Tear Strength, TD | 29.5 g/micron | 750 g/mil | ASTM D1922 |
ExxonMobil NTX™ NTX 141 Super Strength Film Resin NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac.. |
|||
Elmendorf Tear Strength, TD | 29.5 g/micron | 750 g/mil | ASTM D1922 |
ExxonMobil NTX™ NTX 150 Super Strength Film Resin NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac.. |
|||
Elmendorf Tear Strength, TD | 29.5 g/micron | 750 g/mil | ASTM D1922 |
Dow ELITE™ 5220G Enhanced Polyethylene Resin High impact and puncture resistance Excellent on-pallet load elongation for higher yields on regular loads Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |