Polymer Property : Elmendorf Tear Strength, TD = 2.64 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 2.64 g/micron
67.0 g/mil
ASTM D1922
ExxonMobil Escorene® LD-141 EVA Shrink Film Resin, FMI  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 2.0% vinyl acetate copolymer film resin with very good toughness and shrink properties. The low melt index gives excellent..