Polymer Property : Elmendorf Tear Strength, TD = 1.22 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 1.22 g/micron
31.0 g/mil
Calculated from mfr's report of 2.5 N per TAPPI-414 and the typical thickness
DuPont™ Nomex® 411 Paper, 7 mil Nominal Thickness
Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil..