Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 0.700 g/micron | 17.8 g/mil | |
DuPont™ Surlyn® 1601 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1601 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |
|||
Elmendorf Tear Strength, TD | 0.700 g/micron | 17.8 g/mil | |
DuPont™ Surlyn® 1601-2 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1601-2 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, s.. |
|||
Elmendorf Tear Strength, TD | 0.700 g/micron | 17.8 g/mil | |
DuPont™ Surlyn® 1601-2LM Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1601-2LM (Low Moisture) is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications:.. |