Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 0.600 - 1.60 g/micron
15.2 - 40.6 g/mil
Average value: 0.940 g/micron Grade Count:5
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a..