Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 20.5 g/micron
520 g/mil
ASTM D1922
Chevron Phillips Vytek™ V208A Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use..
Elmendorf Tear Strength, MD 20.5 g/micron
520 g/mil
ASTM D1922
Chevron Phillips Vytek™ V208E9 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart drop impact, hot-tack and heat seal properties, good drawdown, can b..