Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 10.0 g/micron | 255 g/mil | ASTM D882 |
Dow INTEGRALâ„¢ 936 High Heat Monolayer Adhesive Film INTEGRAL 936 High Heat Monolayer Adhesive Film is a heat-activated, thermally stable adhesive film for automotive applications capable of bonding to urethane foam-baked fabrics, paper, cardboard, fi.. |