Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 8.925 g/micron | 226.7 g/mil | ASTM D1922 |
ExxonMobil ESCOR™ AT 310 Cast Film Resin
(discontinued **) ESCOR AT 310 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable fo.. |