Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 8.19 g/micron | 208 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-144 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 2% vinyl acetate copolymer packaging film resin. Film made from LD-144 offers improved impact strength and heat sealability compared to homopolym.. |
|||
Elmendorf Tear Strength, MD | 8.20 g/micron | 208 g/mil | ISO 6383-2 |
Total Lumicene® mPE M 2310 EP Metallocene Polyethylene, Blown Film Lumicene® mPE M 2310 EP is a second generation metallocene based Linear Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2310 EP can be processed at high output rates with low ext.. |
|||
Elmendorf Tear Strength, MD | 8.20 g/micron | 208 g/mil | ASTM-D1922 |
Braskem CX7020 LDPE Cast Film Extrusion Polyethylene CX7020 is a low-density polyethylene (LDPE) with excellent processability and low gel content. Those features allow for production of thin and highly uniform films. This product is identified as PE .. |
|||
Elmendorf Tear Strength, MD | 8.19 g/micron | 208 g/mil | ASTM D1922 |
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su.. |
|||
Elmendorf Tear Strength, MD | 8.19 g/micron | 208 g/mil | ASTM D1922 |
ExxonMobil Escorene® LL-3201 LLDPE/Hexene Premium High Strength 1.2 mil Film, Stiff
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope.. |
|||
Elmendorf Tear Strength, MD | 8.19 g/micron | 208 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-331 EVA Film Resin, Very High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.8% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati.. |