Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 0.800 g/micron | 20.3 g/mil | ASTM D1922 |
SABIC F00952 High Density Polyethylene for Blown Film Product Description: F00952 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Elmendorf Tear Strength, MD | 0.800 g/micron | 20.3 g/mil | ASTM D1922 |
SABIC F00952EQ High Density Polyethylene for Blown Film Product Description: F00952EQ is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. the design of the product, molecular architect.. |
|||
Elmendorf Tear Strength, MD | 0.800 g/micron | 20.3 g/mil | ASTM D1922 |
SABIC FJ00952 High Density Polyethylene for Blown Film Product Description: FJ00952 is a TNPP additive free, high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, .. |
|||
Elmendorf Tear Strength, MD | 0.800 g/micron | 20.3 g/mil | ASTM D1922 |
Reliance Industries Relene F46003 Polyethylene Relene F46003 is a High Density Polyethylene grade suitable for producing blown parts with superior stiffness and barrier properties. It is recommended for making liners and coextruded film structu.. |
|||
Elmendorf Tear Strength, MD | 0.800 - 3.94 g/micron | 20.3 - 100 g/mil | Average value: 1.83 g/micron Grade Count:9 |
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m.. |
|||
Elmendorf Tear Strength, MD | 0.800 g/micron | 20.3 g/mil | ASTM D1922 |
Braskem ES 300 HDPE Blown Film Extrusion Polyethylene
(discontinued **) 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags; high-strength films. Informa.. |
|||
Elmendorf Tear Strength, MD | 0.800 g/micron | 20.3 g/mil | ISO 6383-2 |
Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film Lumicene® mPE M 6040 S01 is a second generation metallocene high density polyethylene.Lumicene® mPE M 6040 S01 can be processed at high output rates with low extrusion pressure, low neck-in, excel.. |
|||
Elmendorf Tear Strength, MD | 0.800 g/micron | 20.3 g/mil | ASTM-D1922 |
Braskem LL3800N HDPE Cast Film Extrusion Polyethylene Copolymer The resin LL3800N is a high-density polyethylene, copolymer octene-1, produced by the solution process for the extrusion of plain films with excellent mechanical properties. It has an antirust addit.. |