Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 0.787 g/micron | 20.0 g/mil | ASTM D1922 |
ExxonMobil OPTEMA™ TC 115 Blown Film Resin
(discontinued **) OPTEMA TC 115 is an ethylene methyl acrylate copolymer, designed for specialty blown film applications. It yields soft, elastic films.Information provided by ExxonMobil Chemical |
|||
Elmendorf Tear Strength, MD | 0.787 g/micron | 20.0 g/mil | Notched; ASTM D1922 |
Chevron Phillips HiD® 9640 HDPE Blown Film Resin
(discontinued **) Copolymerization Enhances Film Toughness, Unique Combination of Density and Melt Index, Excellent Strength Properties as well as Good Heat Seal, Lower Density Imparts a Softer Feel and Lesser Tenden.. |
|||
Elmendorf Tear Strength, MD | 0.787 g/micron | 20.0 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD 767.MJ Blown Film Resin
(discontinued **) Escorene Ultra LD 767.MJ is a low gel 29.5% vinyl acetate copolymer designed for film and compounding applications.Information provided by ExxonMobil Chemical |
|||
Elmendorf Tear Strength, MD | 0.787 g/micron | 20.0 g/mil | 1 mil; ASTM D1922 |
Chevron Phillips K-Resin® KR53 Styrene-Butadiene Copolymer Customer Benefits:Excellent ClarityHigh Surface GlossGood ToughnessGood Heat SealabilityTypical Applications:Medical PackagingProduce PackagingTwist WrapLidstock and Labeling FilmInformation provide.. |
|||
Elmendorf Tear Strength, MD | 0.787 g/micron | 20.0 g/mil | Calculated from mfr's report of 1.1 N per TAPPI-414 and the typical thickness |
DuPont™ Nomex® 411 Paper, 5 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Elmendorf Tear Strength, MD | 0.787 g/micron | 20.0 g/mil | Calculated from mfr's report of 1.6 N per TAPPI-414 and the typical thickness |
DuPont™ Nomex® 411 Paper, 7 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Elmendorf Tear Strength, MD | 0.787 g/micron | 20.0 g/mil | ASTM D882 |
Dow XU 66129.00 Developmental Monolayer Adhesive Film XU 66129.00 Developmental Monolayer Adhesive Film is a heat-activated, thermally stable adhesive film capable of bonding to urethane foam-backed fabrics, paper, fiberglass, non-wovens, and rigid ure.. |
|||
Elmendorf Tear Strength, MD | 0.787 - 5.51 g/micron | 20.0 - 140 g/mil | Average value: 4.32 g/micron Grade Count:5 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Film Grade". Each property range of values reported is minimum and m.. |