Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 7.80 g/micron | 198 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® LF-Y320-C Fractional Melt LDPE Film Resin Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL.. |
|||
Elmendorf Tear Strength, MD | 7.80 g/micron | 198 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® LF-Y320-D Fractional Melt LDPE Film Resin Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL.. |
|||
Elmendorf Tear Strength, MD | 7.80 g/micron | 198 g/mil | ASTM D1922 |
Petroquimica Triunfo Trithene® TX 8024 LDPE - High Clarity Film The Trithene TX 8024 resin is a low-density polyethylene (LDPE) with high molecular weight and distribution narrow, designed to obtain films with very high clarity and excellent processability. This.. |