Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 0.394 g/micron
10.0 g/mil
Notched; ASTM D1922
Chevron Phillips HiD® 9606 HDPE Blown Film and Sheet  (discontinued **)
Resin Type: ASTM D 4976 Classification: PE 235, A 54502Applications:General Purpose Films and Sheet, Coextruded Film Structures, Deli and Tissue Films, Sheet Thermoforming Applications with Good Str..
Elmendorf Tear Strength, MD 0.394 - 1.97 g/micron
10.0 - 50.0 g/mil
Honeywell Capran® K Coated Nylon Film  (discontinued **)
Description: Capran® K is a PVdc coated nylon 6 film designed for food packaging applications where longer shelf life is required. This film exhibits good clarity, gloss, toughness, thermoformabil..
Elmendorf Tear Strength, MD 0.394 - 1.97 g/micron
10.0 - 50.0 g/mil
Honeywell Capran® Nylon Film, Multipurpose Nylon 6 Film
Description: Capran® is a multipurpose nylon 6 film. Its physical properties are evenly distributed for optimum performance giving excellent resistance to flex cracking. It can be processed ove..
Elmendorf Tear Strength, MD 0.394 g/micron
10.0 g/mil
Calculated from mfr's report of 1.4 N per TAPPI-414 and the typical thickness
DuPont™ Nomex® 419 Paper, 13 mil Nominal Thickness
Nomex® Type 419 is the uncalendared precursor of Nomex® Type 418. It is used in applications in which its lower density allows improved conformability and saturability.General NOMEX Information: ..
Elmendorf Tear Strength, MD 0.394 g/micron
10.0 g/mil
Calculated from mfr's report of 0.8 N per TAPPI-414 and the typical thickness
DuPont™ Nomex® 419 Paper, 7 mil Nominal Thickness
Nomex® Type 419 is the uncalendared precursor of Nomex® Type 418. It is used in applications in which its lower density allows improved conformability and saturability.General NOMEX Information: ..
Elmendorf Tear Strength, MD 0.394 g/micron
10.0 g/mil
ASTM D1922
ExxonMobil Escorene® HD-7755 HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7755 exhibit excellent impact and toughness properties as well as high stiffness...
Elmendorf Tear Strength, MD 0.394 g/micron
10.0 g/mil
ASTM D1922
ExxonMobil Escorene® HD-7756 HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7756 exhibit excellent impact and toughness properties as well as high stiffness...
Elmendorf Tear Strength, MD 0.394 - 4.21 g/micron
10.0 - 107 g/mil
Average value: 1.86 g/micron Grade Count:4
Overview of materials for Nylon 6, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..