Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 0.394 - 1.97 g/micron | 10.0 - 50.0 g/mil | |
Honeywell Capran® K Coated Nylon Film
(discontinued **) Description: Capran® K is a PVdc coated nylon 6 film designed for food packaging applications where longer shelf life is required. This film exhibits good clarity, gloss, toughness, thermoformabil.. |
|||
Elmendorf Tear Strength, MD | 0.394 - 1.97 g/micron | 10.0 - 50.0 g/mil | |
Honeywell Capran® Nylon Film, Multipurpose Nylon 6 Film Description: Capran® is a multipurpose nylon 6 film. Its physical properties are evenly distributed for optimum performance giving excellent resistance to flex cracking. It can be processed ove.. |