Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 9.21 g/micron | 234 g/mil | ASTM D1922 |
Eastman 1550F Film Polyethylene
(discontinued **) Polyethylene 1550F is a low density polyethylene that contains no additives.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no long.. |