Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 4.92 - 5.31 g/micron | 125 - 135 g/mil | (direction not reported), Propagation Tear Strength; ASTM D-1922 |
Saint-Gobain Norton® PFA Fluoropolymer Film Features/Benefits:Outstanding flex life and stress crack resistancePerformance from -254°C (-425°F) to 260°C (500°F)Outstanding anti-stick release propertiesExcellent electrical properti.. |
|||
Elmendorf Tear Strength, MD | 4.92 g/micron | 125 g/mil | ASTM D1922 |
SCG Chemicals EL-Leneâ„¢ L2020F Linear Low Density Polyethylene Film Key Characteristics:High output and elongationContains 1800 ppm slip agent and 1400 ppm antiblocking agentRecommended Applications:General purpose bag, cast film, small bag, merchandise bag, printed.. |
|||
Elmendorf Tear Strength, MD | 4.92 g/micron | 125 g/mil | Blown Film at 1.25 mil; ASTM D-1922 |
Chevron Phillips MarFlex® 1125 Polyethylene; LDPE Low density polyethylene. This LDPE is tailored for blown film applications that require: Good impactNo slip, includes antiblockGood processabilityGood sealabilityGood drawdown Applications: Typi.. |