Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 3.50 g/micron | 88.9 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® GF-0218-F Butene LLDPE Masterbatch Resin Film Properties. Features: Free flowing granules, toughness and strength, ease of extrusion.Applications: Blending, concentrates.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, MD | 3.50 g/micron | 88.9 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® PF-0218-D Butene LLDPE Film Resin Film Properties. Features: High MI for easier extrusion.Applications: Trash bags, bags-on-roll, garment film.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, MD | 3.50 g/micron | 89.0 g/mil | Average of MD and TD; ASTM D1922 |
DuPont Elvax® 3121A Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
(discontinued **) 7.5 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dr.. |
|||
Elmendorf Tear Strength, MD | 3.50 g/micron | 88.9 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® PF-0218-F Butene LLDPE Film Resin Toughness and strength, Ease of extrusionApplications: Cast films, BlendingAdditives: Process stabilizerFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are depende.. |
|||
Elmendorf Tear Strength, MD | 3.50 g/micron | 88.9 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® PF-0218-J Butene LLDPE Film Resin Film Properties. Features: High MI for easier extrusion.Applications: Trash bags, general purpose packaging, garment film.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, MD | 3.50 g/micron | 88.9 g/mil | |
DuPont™ Surlyn® 1652-1 Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating
(discontinued **) Surlyn® 1652-1 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Elmendorf Tear Strength, MD | 3.50 g/micron | 88.9 g/mil | ISO 6383-2 |
Total EVA 1005 VN 2 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 2 is made by a high pressure tubular process. Grade for transparent and resistant films. Contains an antioxidant.Application examples: Stretch, coextrusion, frozen food, agriculture fi.. |
|||
Elmendorf Tear Strength, MD | 3.50 g/micron | 88.9 g/mil | |
DuPont™ Surlyn® 1652SB Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating Surlyn® 1652SB is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen.. |