Polymer Property : Elmendorf Tear Strength, MD = 16.9 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 16.9 g/micron
430 g/mil
ASTM D1922
ExxonMobil NTX™ NTX 095 Super Strength Film Resin
NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac..
Elmendorf Tear Strength, MD 16.9 g/micron
430 g/mil
ASTM D1922
ExxonMobil NTX™ NTX 104 Super Strength Film Resin
NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac..
Elmendorf Tear Strength, MD 16.9 g/micron
430 g/mil
ASTM D1922
ExxonMobil NTX™ NTX 141 Super Strength Film Resin
NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac..
Elmendorf Tear Strength, MD 16.9 g/micron
430 g/mil
ASTM D1922
ExxonMobil NTX™ NTX 150 Super Strength Film Resin
NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac..
Elmendorf Tear Strength, MD 16.9 g/micron
430 g/mil
ASTM D1922
Dow ELITE™ 5500G Enhanced Polyethylene Resin
™ 5500G is a copolymer produced via INSITE™ Technology. It offers an exceptional combination of processability, low heat seal initiation temperature, package integrity, optical properties, and te..