Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 1.38 g/micron | 35.0 g/mil | ASTM D1922 |
ExxonMobil ESCOR™ AT 320 Blown Film Resin
(discontinued **) ESCOR AT 320 provides excellent adhesion to a variety of substrates and other film components such as aluminum foil, polyolefins, polycarbonate, PET, etc.Information provided by ExxonMobil Chemical |
|||
Elmendorf Tear Strength, MD | 1.38 g/micron | 35.0 g/mil | Notched; ASTM D1922 |
Chevron Phillips HiD® 9605D HDPE Cast Film Resin
(discontinued **) Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical.. |
|||
Elmendorf Tear Strength, MD | 1.38 g/micron | 35.0 g/mil | Notched; ASTM D1922 |
Chevron Phillips HiD® 9607D HDPE Cast Film Resin
(discontinued **) Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical.. |
|||
Elmendorf Tear Strength, MD | 1.38 g/micron | 35.0 g/mil | Notched; ASTM D1922 |
Chevron Phillips MarFlex® 9607XD HDPE Cast Film Resin
(discontinued **) Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical.. |
|||
Elmendorf Tear Strength, MD | 1.38 g/micron | 35.0 g/mil | Notched; ASTM D1922 |
Chevron Phillips MarFlex® 9607 HDPE Cast Film Resin Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical.. |
|||
Elmendorf Tear Strength, MD | 1.38 g/micron | 35.0 g/mil | ASTM D1922 |
ExxonMobil Pax-Plus™ 3201 Blown Film Resin Pax-Plus 3201 is a rubber modified high density polyethylene film resin that exhibits excellent impact strength and stress crack resistance. It is used primarily in film where its good tear resista.. |
|||
Elmendorf Tear Strength, MD | 1.38 g/micron | 35.0 g/mil | ASTM D1922 |
ExxonMobil Pax-Plus™ 3208 Blown Film Resin Pax-Plus 3208 is a rubber modified high density polyethylene film resin offering good physical properties with ease of processing. It exhibits toughness, stress crack resistance and low WVTR.Inform.. |
|||
Elmendorf Tear Strength, MD | 1.38 g/micron | 35.0 g/mil | ASTM D1922 |
Chevron Phillips MarFlex® 9608XD HDPE Film Grade This HDPE is tailored for applications that require:Very low gel levelsVery "clear" filmExcellent drawdownEnhanced stiffnessExcellent WVTR for a chill cast filmExcellent ProcessibilityTypical Cast F.. |