Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 1.20 g/micron | 30.5 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® 20% LF-0718-A in PF-0118-B LDPE Film Resin Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical .. |
|||
Elmendorf Tear Strength, MD | 1.20 g/micron | 30.5 g/mil | |
Dow DOWLEX™ 2027A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2027A Polyethylene resin is a higher density polymer for cast film applications with improved stiffness. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2(a) for food contact appli.. |
|||
Elmendorf Tear Strength, MD | 1.20 g/micron | 30.5 g/mil | |
DuPont™ Surlyn® 2601 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 2601 is an ionomer resin available for use in blown and cast film operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resins. Applicati.. |
|||
Elmendorf Tear Strength, MD | 1.20 - 15.7 g/micron | 30.5 - 400 g/mil | Average value: 7.69 g/micron Grade Count:136 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |