Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 36.70 MPa | 5323 psi | ASTM D882 |
Honeywell Capran® NyLid™ WMB 250 Nylon Lidding Film
(discontinued **) Description: Capran® NyLid™ WMB 250 is a 2.5 mil, white medium barrier nylon co-extruded film with an EVOH core. Applications: Capran® NyLid™ WMB 250 is suitable for die cutting, readily accepts.. |