Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 25.5 MPa | 3700 psi | ASTM D822 |
LyondellBasell Alathon® M6060 High Density Polyethylene ApplicationsALATHON M 6060 is a medium molecular weight high density homopolymer with extremely low gel content. This resin provides high stiffness and narrow molecular weight distribution for use .. |
|||
Film Tensile Strength at Yield, TD | >= 25.5 MPa | >= 3700 psi | ASTM D 882 A |
Total HL 428 HDPE film resin Applications: multi-wall liner, poultry multi-layer gas flush bags, mailing envelopes, heavy-duty shipping sacks, fresh cut produce packaging, coextrusionInformation provided provided by Total Petro.. |