Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 11.7 MPa | 1700 psi | at 2% offset; ASTM D882 |
ExxonMobil Exceed™ 1023CA Tough Premium Film Resin
(discontinued **) Exceed 1023CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1023CA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Film Tensile Strength at Yield, TD | 11.7 MPa | 1700 psi | ASTM D882 |
LyondellBasell Petrothene® M2520FN Low Density Polyethylene ApplicationsPETROTHENE M 2520 is a film grade resin that exhibits excellent optics, good gloss and good bubble stability. A typical application for this resin is high clarity packaging. Regulatory.. |
|||
Film Tensile Strength at Yield, TD | 11.7 MPa | 1700 psi | ASTM D882 |
ExxonMobil Enable™ 23-05HH Metallocene Polyethylene Resin Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Yield, TD | 11.7 MPa | 1700 psi | ASTM D882 |
ExxonMobil Enable™ 23-05NA Metallocene Polyethylene Resin Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Yield, TD | 11.7 MPa | 1700 psi | ASTM D882 |
ExxonMobil LD 123.LN General Purpose Clarity Film Resin Product Description: LD 123.LN blown film grade offers an excellent balance of optical and strength properties for general purpose clear film applications.Availability: Latin America, North America .. |
|||
Film Tensile Strength at Yield, TD | 11.7 MPa | 1700 psi | ASTM D882 |
ExxonMobil LDPE LD 071.LQ Low Density Polyethylene Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
Film Tensile Strength at Yield, TD | 11.7 MPa | 1700 psi | ASTM D882 |
ExxonMobil LDPE LD 071.LR Low Density Polyethylene Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
Film Tensile Strength at Yield, TD | 11.7 MPa | 1700 psi | ASTM D882 |
ExxonMobil LDPE LD 123.LN Low Density Polyethylene Resin Product Description: LD 123.LN blown film grade offers an excellent balance of optical and strength properties for general purpose clear film applications.Availability: Latin America, North America .. |
|||
Film Tensile Strength at Yield, TD | 11.7 MPa | 1700 psi | ASTM D882 |
ExxonMobil LDPE LD 144BR Low Density Polyethylene Resin Product Description: LD 144BR is an LDPE grade, which offers excellent optical properties combined with increased stiffness and drawdown properties.Availability: Africa & Middle East and Europe Addi.. |
|||
Film Tensile Strength at Yield, TD | 11.7 MPa | 1700 psi | ASTM D882 |
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin Product Description: LD 165BW1 is a fractional melt index LDPE, with medium optical properties.Availability: Latin America, North America and South America Applications: Agricultural FilmBlend Part.. |
|||
Film Tensile Strength at Yield, TD | 11.7 MPa | 1700 psi | |
Dow DOWLEX™ 2032 Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2032 Polyethylene resin is a general purpose liner resin having improved thermal stability over a broad range of processing conditions. It is an outstanding choice for thin gauge, medium st.. |