Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 8.00 MPa | 1160 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-0219-E Hexene LLDPE Film Resin Exceptional toughens, Low gel levelApplications: Cast stretch wrapAdditives: High temperature A/OFilm properties are typical of cast film extruded at a melt temperature of 540°F, and a line speed o.. |
|||
Film Tensile Strength at Yield, TD | 8.00 MPa | 1160 psi | ISO 527-3 |
Polimeri Europa Flexirene® CL 10 Butene Copolymer Linear Low Density Polyethylene Flexirene CL 10 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for cast extrusion of thin film with high optical properties.Main Applications: Flexire.. |
|||
Film Tensile Strength at Yield, TD | 8.00 MPa | 1160 psi | ISO 527-3 |
Polimeri Europa Greenflex® FD 20 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 20 is an ethylene vinyl acetate copolymer (EVA) suitable for blown film extrusion. Films produced with Greenflex FD 20 exhibit good optical properties, high impact resistance, tensile .. |
|||
Film Tensile Strength at Yield, TD | 8.00 MPa | 1160 psi | ISO 527-3 |
Polimeri Europa Greenflex® FD 23 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 23 is an ethylene vinyl acetate copolymer (EVA) suitable for blown film extrusion. Greenflex FD 23 is a version of Greenflex FD 20 with added slip and antiblocking agents. Films produ.. |
|||
Film Tensile Strength at Yield, TD | 8.00 MPa | 1160 psi | ASTM D882 |
Westlake Mxsten CV CV77515-F Plastomer
(discontinued **) Mxsten CV plastomer CV77515-X is a polyethylene plastomer designed for blown film extrusion that contains medium slip and no antiblock additives. Films produced with this resin exhibit a very low s.. |
|||
Film Tensile Strength at Yield, TD | 8.00 - 18.0 MPa | 1160 - 2610 psi | Average value: 10.9 MPa Grade Count:48 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum.. |
|||
Film Tensile Strength at Yield, TD | 8.00 MPa | 1160 psi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ L2020F Linear Low Density Polyethylene Film Key Characteristics:High output and elongationContains 1800 ppm slip agent and 1400 ppm antiblocking agentRecommended Applications:General purpose bag, cast film, small bag, merchandise bag, printed.. |
|||
Film Tensile Strength at Yield, TD | 8.00 MPa | 1160 psi | ASTM D882 |
Westlake Mxsten CV77512 Polyethylene Plastomer Mxsten CV plastomer CV77512 is a polyethylene plastomer designed for blown film extrusion that contains high slip, high antiblock and high processing aid additives. Films produced with this resin ex.. |
|||
Film Tensile Strength at Yield, TD | 8.00 MPa | 1160 psi | ASTM-D882 |
Westlake Mxsten CV77519 Polyethylene Plastomer Mxsten CV Plastomer CV77519 is a polyethylene plastomer designed for blown film extrusion that contains no slip and no antiblock. It does contain high processing aid. Films produced with this resin .. |
|||
Film Tensile Strength at Yield, TD | 8.00 MPa | 1160 psi | 2 in per min; ASTM D882 |
Chevron Phillips MarFlex® D143 m-LLDPE Linear Low Density Polyethylene Low Density PolyethyleneCustomer Benefits: This metallocene LLDPE film resin possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved proce.. |
|||
Film Tensile Strength at Yield, TD | 8.00 MPa | 1160 psi | ASTM D882 |
ExxonMobil Escorene® LL-3003 LLDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3003 have outstanding tensile properties as well as stiffness and toughness.Applicatio.. |