Mechanical Properties Metric English Comments
Shear Modulus 3.47 - 3.88 GPa
503 - 563 ksi
Calculated
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)  (discontinued **)
Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten..