Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 6.30 GPa | 914 ksi | in <110> direction |
Mateck Potassium Chloride (KCl) Optical crystals |
|||
Shear Modulus | 6.30 GPa | 914 ksi | |
Specialty Materials 5505 Boron Epoxy Prepreg Tape Specialty Materials' 5505 is a highly advanced prepreg tape, combining Specialty Materials' 4.0 or 5.6 mil boron filament with a tough, rigid, epoxy resin. Exhibiting exceptional performance at temp.. |
|||
Shear Modulus | 6.30 GPa | 914 ksi | |
Specialty Materials 5521 Boron Epoxy Prepreg Tape Specialty Materials' 5521 is a highly advanced prepreg tape, combining Specialty Materials' 4.0 or 5.6 mil boron filament with a tough, rigid, epoxy resin. Performing at temperatures up to 350°F,.. |