Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 5.96 - 6.10 GPa | 864 - 885 ksi | Calculated |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |