Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 58.9 GPa | 8540 ksi | Calculated |
Carpenter Super Invar 32-5 Carpenter Super Invar 32-5, a magnetic, austenitic, solid solution alloy containing iron, nickel and cobalt, is designed to provide minimum thermal expansion at room temperatures. This alloy also e.. |