Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.565 GPa | 81.9 ksi | DIN 53457 |
Global PP-2540-K Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-paint drum, storage & transport containerInformation provided by Global Polymers Corporation. |