Mechanical Properties Metric English Comments
Shear Modulus 50.0 GPa
7250 ksi
Calculated
Osprey Metals CE7 Al-Si Controlled Expansion Alloy
Si-30%Al controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals.
Shear Modulus 50.0 GPa
7250 ksi
Meehanite GC-40 Flake Graphite Cast Iron
Type GC-40 combines good strength with low coefficient of friction and self lubricating properties. It is easily machinable with a fine, dense, close grain structure. Recommended for heavy brake d..
Shear Modulus 50.0 GPa
7250 ksi
CeramTec 447 Cordierite, 2MgO•Al2O3•5SiO2
Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c..