Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 5.00 GPa | 725 ksi | Calculated |
Premix Premi-Glas® 3101-20 Polyester BMC Premi-Glas® 3101-20 a 20% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL 94-.. |
|||
Shear Modulus | 5.00 GPa | 725 ksi | in plane |
Menzolit Menzolit® BMC 0160 Unsaturated Polyester UP BMC 0160 is a general purpose BMC for electrical applications. Typical applications are lamp housings, canopies, covers and similar components.Information Provided by Menzolit |
|||
Shear Modulus | 5.00 GPa | 725 ksi | in plane |
Menzolit Menzolit® BMC 0170 Unsaturated Polyester UP BMC 0170 is a general purpose BMC for electrical applications. Product according to type 801 DIN 16911. The glass content is on a level that combines good mouldability with good strength and stiffne.. |
|||
Shear Modulus | 5.00 GPa | 725 ksi | in plane |
Menzolit Menzolit® BMC 0180 Unsaturated Polyester UP BMC 0180 is a general purpose BMC for electrical applications. Product according to type 803 DIN 16911. The glass content is on a level that combines good mould ability with good strength and stiffn.. |
|||
Shear Modulus | 5.00 GPa | 725 ksi | in plane |
Menzolit Menzolit® BMC 0200 Unsaturated Polyester UP BMC 0200 is a standard BMC for general purpose applications. The glass content is on a level that combines good mouldability with good strength and stiffness properties. Even without a specific fire.. |
|||
Shear Modulus | 5.00 GPa | 725 ksi | in plane |
Menzolit Menzolit® BMC 0800 Unsaturated Polyester UP BMC 0800 is a special SMC for applications within household and kitchenware. The glass level has been selected to combine good mould ability with good strength and stiffness properties. The product .. |
|||
Shear Modulus | 5.00 GPa | 725 ksi | in plane |
Menzolit Menzolit® BMC 0900 Unsaturated Polyester UP BMC 0900 is a special BMC used in a chemically aggressive environment. The glass content is set to a level that combines good mould ability with good strength and stiffness properties. Typical appli.. |
|||
Shear Modulus | 5.00 GPa | 725 ksi | in plane |
Menzolit Menzolit® BMC 1000 Unsaturated Polyester UP BMC 1000 is a special BMC for hydrolysis resistant applications. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. Typical applic.. |
|||
Shear Modulus | 5.00 GPa | 725 ksi | in plane |
Menzolit Menzolit® BMC 1100 Unsaturated Polyester UP BMC 1100 is a special BMC for high strength application. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. The selection of the r.. |
|||
Shear Modulus | 5.00 GPa | 725 ksi | in plane |
Menzolit Menzolit® BMC 1650 Unsaturated Polyester UP BMC 1650 is a specially designed anti-microbial polyester moulding compound which incorporates a "germ killer" . It has been tested and found to be compliant for resistance to fungal defacement in .. |
|||
Shear Modulus | 5.00 GPa | 725 ksi | in plane |
Menzolit Menzolit® BMC 2500 Unsaturated Polyester UP BMC 2500 is a special BMC for high voltage isolating applications. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. The fire retardanc.. |
|||
Shear Modulus | 5.00 GPa | 725 ksi | in plane |
Menzolit Menzolit® SMC 1100 Unsaturated Polyester UP SMC 1100 is a special vinylester SMC for high strength applications. The reinforcement has been put to a level that combines mouldability with high strength and stiffness properties. The specific re.. |
|||
Shear Modulus | 5.00 GPa | 725 ksi | in plane |
Menzolit Menzolit® BMC 0190 Unsaturated Polyester UP BMC 0190 is a general purpose BMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The flammability me.. |
|||
Shear Modulus | 5.00 GPa | 725 ksi | in plane |
Menzolit Menzolit® BMC 0300 Unsaturated Polyester UP BMC 0300 is a low shrink standard material for general-purpose applications, which require a higher level on surface quality and better dimensional stability. The glass content is on a level that co.. |
|||
Shear Modulus | 5.00 GPa | 725 ksi | in plane |
Menzolit Menzolit® BMC 1400 Unsaturated Polyester UP BMC 1400 is a special BMC for the use on an engine. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. The product has been developped f.. |
|||
Shear Modulus | 5.00 GPa | 725 ksi | in plane |
Menzolit Menzolit® BMC 2300 Unsaturated Polyester UP BMC 2300 is a special BMC with exceptional high fire retardancy. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. Fire retardanc.. |
|||
Shear Modulus | 5.00 GPa | 725 ksi | in plane |
Menzolit Menzolit® BMC 2600 Unsaturated Polyester UP BMC 2600 is a special BMC with reduced electrical properties. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. Because of its improved.. |
|||
Shear Modulus | 5.00 GPa | 725 ksi | in plane |
Menzolit Menzolit® BMC 2910 Unsaturated Polyester UP BMC 2910 incorporates additives which enhance the integral performance of mouldings during and after fire, currently used to mould Boltcaps which are designed to provide protection to the bolted co.. |
|||
Shear Modulus | 5.00 GPa | 725 ksi | In Plane |
Goodfellow Carbon/Epoxy Composite Sheet Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow. |
|||
Shear Modulus | 5.00 GPa | 725 ksi | In-Plane; After ageing at 70°C / 95% RH; RT |
Hexcel® HexPly® 922-1/35%/G926 180°C Curing Epoxy Matrix 5H satin/370g/m2 carbon fabric: FVC=60%Information provided by HexCel |
|||
Shear Modulus | 5.00 GPa | 725 ksi | calculated |
BASF Capron® 8234G 44% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8234G is a 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is .. |