Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 37.7 GPa | 5470 ksi | Calculated |
CRP Technology 8601 Aerospace Grade Power Metallurgy Aluminum Alloy For Motorsport and Aerospace marketplaces: manufactured by a special powder metallurgy process using a high-energy mixing process which ensures excellent mechanical properties.Super Aluminium materi.. |