Mechanical Properties Metric English Comments
Shear Modulus 0.0365 GPa
5.30 ksi
Plate Shear, L Direction, preliminary value obtained from limited testing
Hexcel® HexWeb® HRH-78 - 1/8 - 3.0 Commercial Grade Nomex Honeycomb/Phenolic Resin
Designation: Material-Cell Size (inches)-DensityHexWeb HRH-78 is manufactured from commercial grade aramid paper sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after..
Shear Modulus 0.0365 GPa
5.30 ksi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRP - 3/8 - 3.5 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..