Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 2.91 GPa | 422 ksi | Calculated |
Plenco 7467 Phenolic, Nodular, Transfer Molded
(discontinued **) Two-Stage Phenolic. PLENCO 07467 is an organic phenolic molding compound offering excellent dimensional stability under conditions of total water immersion. 07467 is formulated to provide improved .. |