Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 152 GPa | 22000 ksi | Calculated |
CoorsTek AD-995 Alumina (nom. 99.5% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Shear Modulus | 152 GPa | 22000 ksi | Calculated |
CoorsTek AD-996 99.6% Alumina |
|||
Shear Modulus | 152 GPa | 22000 ksi | Calculated |
CoorsTek AD-998 Alumina(nom. 99.8% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Shear Modulus | 152 GPa | 22000 ksi | Calculated |
CoorsTek CAP 3 99.5% Alumina Ceramic Armor Material CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys.. |
|||
Shear Modulus | 152 GPa | 22000 ksi | Calculated |
CoorsTek PlasmaPure™ Alumina (nom. 99.8% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |