Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 146 GPa | 21200 ksi | Calculated |
CeramTec DN 70 Dispersion Ceramic, Al2O3-ZrO2 DN 70 is a ZTA Alumina Toughened Zirconia. |
|||
Shear Modulus | 146 GPa | 21200 ksi | Calculated |
CoorsTek Zirconia-Toughened Alumina, ZTA Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Shear Modulus | 146 GPa | 21200 ksi | Calculated |
CeramTec B 40 Alumina, 99.1% B 40 is the ideal sliding mate with the same properties as Rubalit® A 1896. It contains a larger share of Al2O3 for superior chemical stability. |