Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.32 - 1.44 GPa | 191 - 209 ksi | Calculated |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz.. |
|||
Shear Modulus | 1.32 - 4.10 GPa | 191 - 595 ksi | Average value: 2.61 GPa Grade Count:8 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |