Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0931 GPa | 13.5 ksi | Plate Shear, L Direction, typical value |
Hexcel® HexWeb® HRH-36® Flex-Core® HRH-36 - F50 - 3.0 Aramid Honeycomb Designation: Material-Cell Size (cells per lineal foot in W direction)-Density (lb per cubic foot)HexWeb HRH-36 Flex-Core aramid paper is reinforced with a high temperature phenolic resin. This prod.. |
|||
Shear Modulus | 0.0931 GPa | 13.5 ksi | Plate Shear, L Direction, typ, preliminary value obtained from limited testing |
Hexcel® HexWeb® CFC™-20-1/8-6.0 Composite Flooring Honeycomb Core Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp.. |