Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0896 GPa | 13.0 ksi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRH-10 - 3/16 - 6.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Modulus | 0.0896 GPa | 13.0 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRH-327 - 3/8 - 5.5 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Shear Modulus | 0.0896 GPa | 13.0 ksi | Plate Shear, W Direction |
Hexcel® HexWeb® HRH-36 - 1/8 - 6.0 Para-Aramid/Phenolic Core Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low.. |
|||
Shear Modulus | 0.0896 GPa | 13.0 ksi | Plate Shear, L Direction, preliminary value obtained from limited testing |
Hexcel® HexWeb® HRH-78 - 3/16 - 6.0 Commercial Grade Nomex Honeycomb/Phenolic Resin Designation: Material-Cell Size (inches)-DensityHexWeb HRH-78 is manufactured from commercial grade aramid paper sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after.. |
|||
Shear Modulus | 0.0896 GPa | 13.0 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRP - 1/4 - 6.5 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Modulus | 0.0896 GPa | 13.0 ksi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRP - 3/16 - 4.0 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Modulus | 0.0896 GPa | 13.0 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRP/F50 - 4.5 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo.. |
|||
Shear Modulus | 0.0896 GPa | 13.0 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR III 3/16-5056-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Modulus | 0.0896 GPa | 13.0 ksi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRH-10 - 1/8- 6.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |