Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.00690 GPa | 1.00 ksi | Typical; ASTM C273 |
Parabeam Industrie Paraglass 12 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |
|||
Shear Modulus | >= 0.00689 GPa | >= 1.00 ksi | Plate Shear, W Direction, minimum individual |
Hexcel® HexWeb® HRH-310 - 1/8 - 1.8 Aramid Fiber/Polyimide Resin Honeycomb Designation: Material-Cell Size-DensityHexWeb HRH-310 is manufactured from aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the hexagon.. |