Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | >= 0.000800 GPa | >= 0.116 ksi | ASTM C273 |
Parabeam Industrie Paraglass 18 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |
|||
Shear Modulus | 0.000800 GPa | 0.116 ksi | Typical; ASTM C273 |
Parabeam Industrie Paraglass 22 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |