Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.000448 GPa | 0.0650 ksi | ASTM D 1002 |
Arlon Thermabond® R36300W008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Low Outgassing, Thermally Conductive, Electrically Insulating, Thermabond® Bonds without primerRecommended Primers: Dow Corning S2260Design/Construction: Liner: FEP Product: Uncured S.. |
|||
Shear Modulus | 0.000448 GPa | 0.0650 ksi | ASTM D 1002 |
Arlon Thermabond® R36300W015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Corning S2260Appearance: White silicone gumThis data represents typical val.. |
|||
Shear Modulus | 0.000448 GPa | 0.0650 ksi | ASTM D1002 |
Arlon Thermabond® T-20 NP (99770W008) 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: 8 mil Primerless Thermabond®. T-20 NP. Thermally conductive, electrically insulating electronic adhesive. Bonds with primer.Design/Construction: Liner: FEP Product: Uncured Silicone Ru.. |
|||
Shear Modulus | 0.000448 GPa | 0.0650 ksi | ASTM D1002 |
Arlon Thermabond® T-20 NP (99770W015) 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: 15 mil Primerless Thermabond®. T-20 NP. Thermally conductive, electrically insulating electronic adhesive. Bonds with primer.Design/Construction:Liner: FEPProduct: Uncured Silicone Rub.. |